Units
Test method
For WC, weigh the cylinder empty and full, dried on the outside. Read the burette with the pump piston in the same, back, position every time; a litre of water counts as a kilogram.
The design standard sets the limit: 10 % for steel to ISO-9809-1 and ISO-9809-3, 5 % for high-strength steel (ISO-9809-2, 1,100 MPa and more) and aluminium (ISO-7866). All parts of BS-5045, steel or aluminium, use 5 %; DOT cylinders, steel or aluminium, are rejected above 10 % at requalification. If the design standard isn't known, ISO-18119 applies 5 %.